Title: Wear Mechanisms of Piston Seals for reciprocating handpumps for rural water supply Authors: M. Lubwama, K. Sayers, J.B. Kirabira, B. Corcoran Keywords: First level surface analysis; Piston seals; Reciprocating handpump; Rural drinking water supply; Wear mechanisms Issue Date: 2011 Abstract: In Uganda 63% of the rural population depend on improved water sources for drinking...Read More